US12569598USUSPTO Grant XML

Method for preparing poly (thioctic acid)-copper coating on surface of cardiovascular stent material

A method for preparing a poly(thioctic acid)-copper coating (poly(TA-Cu)) on a surface of a cardiovascular stent material includes: grinding a cardiovascular stent material with sandpaper until the surface of the cardiovascular stent material is flat and smooth, rinsing the cardiovascular stent material with deionized water and anhydrous ethanol in sequence, and drying the cardiovascular stent material to obtain a pre-treated cardiovascular stent material; dissolving thioctic acid in an alcoholic solvent, adding anhydrous copper chloride to a mixed solution of thioctic acid and the alcoholic solvent, stirring the mixed solution, to yield a precursor solution; treating the pre-treated cardiovascular stent material with the precursor solution, and drying, thus forming a poly(thioctic acid)-copper coating on the surface of the pre-treated cardiovascular stent material. The concentration of thioctic acid in the alcoholic solvent is 0.1-0.3 g/mL, and the molar ratio of anhydrous copper chloride to thioctic acid monomer is 1:100-5000.

Patent

Brief

Patent brief

Problem

How can corrosion in underground pipelines and conduits be prevented?

Novelty

The concentration of thioctic acid in the alcoholic solvent is 0.1-0.3 g/mL, and the molar ratio of anhydrous copper chl...

Uses

Underground pipe, Metal conduit, Industrial line

Assignee

ZHENGZHOU UNIVERSITY

Published

Mar 10, 2026

Inventors

Shaokang Guan, Zhaoqi Zhang, Jingan Li, Shijie Zhu, Liguo Wang, Peiduo Tong, Yahui Wang

Domain

Infrastructure / energy

Plain-English summary

Problem

How can corrosion in underground pipelines and conduits be prevented?

Solution

method for preparing a poly(thioctic acid)-copper coating (poly(TA-Cu)) on a surface of a cardiovascular stent material includes: grinding a cardiovascular stent material with sandpaper until the surface of the cardiovascular stent material is flat and smooth, rinsing the cardiovascular stent material with deionized water and anhydrous ethanol in sequence, and drying the cardiovascular stent material to obtain a pre-treated cardiovascular stent material; dissolving thioctic acid in an alcoholic solvent, adding anhydrous copper chloride to a mixed solution of thioctic acid and the alcoholic solvent, stirring the mixed solution, to yield a precursor solution; treating the pre-treated cardiovascular stent material with the precursor solution, and drying, thus forming a poly(thioctic acid)-copper coating on the surface of the pre-treated cardiovascular stent material.

Key novelty

The concentration of thioctic acid in the alcoholic solvent is 0.1-0.3 g/mL, and the molar ratio of anhydrous copper chloride to thioctic acid monomer is 1:100-5000.

Applications

Underground pipeMetal conduitIndustrial line

Relevant search intents

coating

Related patents